What are you guys using for satin finish blazing gun parts?
And where from
Glass beads from The Tool Shed. Regulate the pressure to get different levels of satin on different materials. For example, I find 30-40psi is plenty for a fine satin on aluminum before anodizing. More like 60-70psi for stainless.
so...this water trap that is mentioned.....I assume thats a bit like a pot smokers bong??? air/dust is sucked through water trap and the particles are trapped in water to reuse later???
I suspect he means keeping the compressed air dry to avoiding clumping/clogging.